Al-Pd-Co复杂合金相压痕形变结构的电子显微学研究
于海涛,刘翠秀,周玲玲,李万鹏,孙 威*
(北京工业大学固体微结构与性能研究所,北京 100024)
摘要 本文以Al-Pd-Co复杂合金相ξ’为研究对象,应用FIB技术以及透射电镜,对其室温下的纳米压痕变形微观结构进行了分析表征。结果表明,不同于传统材料的变形,ξ’相压痕下的变形结构以形成的特殊变形带结构为主要特征。这种变形带由高密度缺陷的集合组成,其在形变过程中可协调局域变形,分割晶粒,且其拓展可以选择沿某些晶体学方位优先开动。
关键词 Al-Pd-Co合金; 复杂合金相;纳米压痕;变形结构;电子显微表征
中图分类号:TG146;TG115.5;TG115.21+5.3 文献标识码:A doi:10.3969/j.issn.1000-6281.2017.04.008
Electron microscopy study of indentation deformation structure of Al-Pd-Co complex alloy phase
YU Hai-tao,LIU Cui-xiu,ZHOU Ling-ling,LI Wan-peng,SUN Wei*
(Institute of Microstructure and Properties of Advanced Material Beijing University of Technology,Beijing 100024,China)
Abstract In this paper, the room-temperature nanoindentation-induced deformation structure in the Al-Pd-Co complex alloy phase ξ’ has been studied by a combination of FIB fabrication technique and electron microscopy. The results show that, unlike the case in a traditional material, the evolution of deformation structure beneath an indent in the ξ’ phase is characterized by the formation of a kind of special deformation band. This kind of deformation band, which can propagate preferentially along some crystallographic planes, is constructed by coupling deformation defects of high density, and its generation and extension are responsible for accommodating plastic strain and for subdividing grain as well during the indentation process.
Keywords Al-Pd-Co;complex alloy phase;nanoindentation;deformation structure;electron microscopy
全文下载请到同方知网、万方数据库或重庆维普等数据库中下载!
[1]SHECHTMAN D, BLECH I, GRATIAS D, et al. Metallic phase with long-range orientational order and no translational symmetry[J]. Physical Review Letters, 1984, 53(20): 1951.
[2] JANOT C. Conductivity in quasicrystals via hierarchically variable-range hopping[J]. Physical Review B, 1996, 53(1): 181.
[3] BILUSIC A, BUDROVI Z, SMONTARA A, et al. Transport properties of icosahedral quasicrystal Al 72 Pd 19.5 Mn 8.5[J]. Journal of Alloys and Compounds,2002,342(1): 413-415.
[4] 董闯. 准晶材料的形成机制, 性能及应用前景[J]. 材料研究学报, 1994, 8(6): 481-490.
[5] 丁棣华, 王仁卉. 准晶的弹性, 塑性与位错[J]. 物理学进展, 1998, 18(3): 223-260.
[6] 李志强, 徐洲, 李小平, 等. 准晶材料的应用研究进展[J]. 材料导报, 2002, 16(2): 9-11.
[7] 陈永君, 胡小刚, 羌建兵, 等. 准晶磨料的“碾抹” 特性对软金属表面的平整性, 硬度及耐蚀性的影响[J]. 金属学报, 2016, 52(10): 1353-1362.
[8] BOISSIEU M, DURAND-CHARRE M, BASTTE P, et al. Centimetre-size single grain of the perfect Al-Pd-Mn icosahedral phase[J]. Philosophical Magazine Letters, 1992, 65(3): 147-153.
[9] BOUDARD M, BOURGEAT-LAMI E, BOISSIEU M, et al. Production and characterization of single quasicrystals of the Al-Pd-Mn icosahedral phase[J]. Philosophical Magazine Letters, 1995, 71(1): 11-19.
[10] WOLLGARTEN M, BEYSS M, URBAN K, et al. Direct evidence for plastic deformation of quasicrystals by means of a dislocation mechanism[J]. Physical Review Letters, 1993, 71(4): 549-552.
[11] 刘镇洋,孙威. 凝固冷却速率影响下Al-Pd-Co复杂合金相的形成及分布特征[J].电子显微学报, 2010, 29(4): 311-316.
[12] YUBUTA K, SUN W, HIRAGA K. A new crystalline phase related to decagonal quasicrystals with non-central symmetry in Al- Co-Pd alloys[J]. Philosophical Magazine A, 1997, 75(1): 273-284.
[13] YURECHKO M, GRUSHKO B, VELIKANOVA T, et al. Isothermal sections of the Al-Pd-Co alloy system for (50~100) at.% Al [J]. Journal of Alloys and Compounds, 2002, 337(1): 172-181.
[14] YURECHKO M, GRUSHKO B, VELIKANOVA T Y, et al. A comparative study of the Al-Co-Pd and Al-Co-Ni alloy systems[J]. Journal of Alloys and Compounds, 2004, 367(1): 20-24.
[15] SUN W, WANG J P, ZHANG Z. Structural defects in Al-Ni-Rh and Al-Pd-Fe crystalline approximant phases[J]. Zeitschrift für Kristallographie International Journal for Structural, Physical, and Chemical Aspects of Crystalline Materials, 2009, 224(1/2): 75-78.
[16] 王瑞萍,孙威,周玲玲. 急冷Al-Cu-Cr合金中二十面体准晶-晶体相变的原位TEM研究[J].电子显微学报,2015,34(5):395-400.
[17] REIBOLD M, BELGER A, MUKHOPADHYAY N K, et al. The impact of nanoindentation at room temperature upon the real structure of decagonal AlCoNi quasicrystals[J]. Physica Status Solidi (A), 2005, 202(12): 2267-2276.
[18] 张琼, 周海芳, 李斗星. 室温下单晶硅压痕微裂纹的形成与扩展[J]. 电子显微学报, 2002, 21(1): 56-58.
[19] JANG J, PHARR G M. Influence of indenter angle on cracking in Si and Ge during nanoindentation[J]. Acta Materialia, 2008, 56(16): 4458-4469.